ABS has slightly lower (10-15%) tensile strength than PLA, a... En el foro Print tips (Archive) |
hace 7 years | |
Crap, apparently there is a time limit on editing posts... I... En el foro Print tips (Archive) |
hace 7 years | |
D'oh, I should add one more thing: for those importing the ... En el foro Print tips (Archive) |
hace 7 years | |
I'm using a 0.4 nozzle, which should be set in the Slic3r se... En el foro Print tips (Archive) |
hace 7 years | |
Polycarbonate: Here's how to print it without warping, delam... En el foro Print tips (Archive) |
hace 7 years | |
Glass transition temperatures: not what they seem En el foro Print tips (Archive) |
hace 7 years |