Drooping layers
i went from prusament to matchbox pls, just used stock prusament settings.
Pics maybe upside down.
Nozzle too hot?
Sorry, pla, not pls.
Mk3 - 1X
Mk3S - 2X
2021 Hyundai Palisade
Wife - 1X
RE: Drooping layers
I hope this is oriented properly.
Mk3 - 1X
Mk3S - 2X
2021 Hyundai Palisade
Wife - 1X
RE: Drooping layers
Yup, overhang is too steep & printing too hot. Note prusament prints hotter than most normal PLAs, you'll want to use the generic PLA profile and probably tweak the temperatures from there.
RE: Drooping layers
You can also slow down print speed to allow more time between layers, especially slow the perimeter speeds to allow more time for the filament to cool between layers. Something like 20mm/s or even 15mm/s.