Avisos
Vaciar todo
Drooping layers
i went from prusament to matchbox pls, just used stock prusament settings.
Pics maybe upside down.
Nozzle too hot?
Sorry, pla, not pls.
Este debate ha sido modificado el hace 5 years por Joey
Mk3 - 1X
Mk3S - 2X
2021 Hyundai Palisade
Wife - 1X
Respondido : 30/05/2019 8:46 pm
Topic starter
answered:
RE: Drooping layers
I hope this is oriented properly.
Attachment removed
It seems it isn't. Why me???
Esta publicación ha sido modificada el hace 5 years por Joey
Mk3 - 1X
Mk3S - 2X
2021 Hyundai Palisade
Wife - 1X
Respondido : 30/05/2019 9:00 pm
RE: Drooping layers
Yup, overhang is too steep & printing too hot. Note prusament prints hotter than most normal PLAs, you'll want to use the generic PLA profile and probably tweak the temperatures from there.
Respondido : 30/05/2019 10:02 pm
RE: Drooping layers
You can also slow down print speed to allow more time between layers, especially slow the perimeter speeds to allow more time for the filament to cool between layers. Something like 20mm/s or even 15mm/s.
Optionally, add a delay between layers to let things cool before adding more hot material.
Esta publicación ha sido modificada el hace 5 years por --
Respondido : 31/05/2019 2:56 am