hello! i have a Prusa XL with a V6 adapter and a CHT Hardened steel nozzle attached.
despite multiple cleanings and cold pulls, it still seems to clogg after about an hour of printing, is this possibly a temp problem? i have the temp at 215 C with PLA filiment
Publié : 13/07/2024 8:58 pm
Different nozzle materials do propagate heat differently - steel *tends* to require a few degrees higher printing temperature.
Try 5°C higher, or even 10.
Cheerio,
Publié : 13/07/2024 9:56 pm
Topic starter
answered:
RE: Clogging with harden steel CHT nozzle
so i did attempt this while typing this out, it sadly failed horribly
Publié : 13/07/2024 10:15 pm
Which filament? What nozzle diameter? Picture of failed print?
Cheerio,
Publié : 14/07/2024 6:38 pm