Printing tubes Seam issues
MINI+
PETG (White)
When printing a tube with only one layer thickness I have to set Extra length on restart to 0.5 (at least) to have the seam join and not cause a gap. That causes a bump if the he model is thicker/round with less or no hole in the middle.
When printing single wall the start of the layer gets more filament than the end as seen in photo.
Settings: 0.4 Nozzle, PETG, Extra Length on restart 0.5, Extruder multiplier 1.01
RE: Printing tubes Seam issues
This might help you. Look at the random seam
https://help.prusa3d.com/article/seam-position_151069
--------------------
Chuck H
3D Printer Review Blog
RE: Printing tubes Seam issues
If it's a single perimeter wide wall, would vase mode work for you? No seams.
Formerly known on this forum as @fuchsr -- until all hell broke loose with the forum software...
RE: Printing tubes Seam issues
Sadly not an option this print is only to dial in the settings without wasting plastic.
RE: Printing tubes Seam issues
Random seam is not an option, at least not until calibrated to almost perfection. After reading the link I am pretty sure this is related to Linear Advance