RE: Persisting oozing blobs and stringing with Prusament PETG - What am I doing wrong?
I was about to say the same thing when my brand new Prusa Mini didn't print as I expected it. Blobs and strings like hell while this file prints fine on my MKS3s. Neon Green Prusament PETG always stored in plastic bag. Guess I'll order a drybox to see if that helps. Never have this problem with 100s of PLA prints, but not with this PETG some six months ago either.
RE: Persisting oozing blobs and stringing with Prusament PETG - What am I doing wrong?
I'm also convinced that Mini's and PETG do not go well together. Great results, low rejects with MK3, lots of boogers and excessive reject rate with Mini.
RE: Persisting oozing blobs and stringing with Prusament PETG - What am I doing wrong?
I guess YMMV. I don't seem to have many issues with PETG on my Minis. But Neon Green is definitely a bitch, without excessive drying it is hard to print on my Mk3S or Minis.
Formerly known on this forum as @fuchsr -- until all hell broke loose with the forum software...
RE: Persisting oozing blobs and stringing with Prusament PETG - What am I doing wrong?
I use Overture PETG black on my stock mini with pretty good results. I changed the Generic PETG profile by reducing nozzle temp from 240 to 225. I do get a random blob from time to time though.