Notifications
Clear all

Perfect surface layer after support (ASA)  

  RSS
EBS
 EBS
(@ebs)
Active Member
Perfect surface layer after support (ASA)

Hi guys.

I have recessed (Z-axis) flat pockets where there will be sealings later on. Unfortunately the surface is far from great. Up to now I had no success with soluble interfaces but will try again with Verbatim BVOH soon. Any idea how to improve the quality of the first layer after the support? Something like ironing would be great I guess but there is no paint on ironing yet.

By the way: the soluble print settings mess around with the filament settings in the printer. After such an print - using soluble full with self designed blocks underneath, Extruder 1 is set to the filament of Extruder 2 (the support material). It has to be changed prior to the next print by changing filament.

Posted : 21/02/2024 10:36 am
Share: