Hello Guys,
I made the upgrade from MK3 to MK3S yesterday.
Oh boy, it took quite some time but it was very interesting to disassemble and to reassemble everything.
Before I did the upgrade, I switched back from the nyloc method of bed leveling correction to the original version with spacers.
I felt, that i somehow didnt do it correctly. So, I wanted a clean and fresh start.
Current Situation: MK3S Upgrade, heatbed mounted on spacers and I use the power coated sheet.
Live Z Value: -1.330
First Layer Calibration:
Prusa Mesh Leveling:
What do you guys suggest?
1. Nyloc Method
2. Spring Method
3. Bed Leveling Correction via printer
4. Playing only with Live Z
5. Something else...?
I do have some spare nyloc nuts, so I "could" do the nyloc method again. But I am also open for other suggestions.
Thank you guys in advance :).
RE: MK3S -> First Layer Calibration Issue -> with Poweder Coated Sheet
Surface Smoothness:
RE: MK3S -> First Layer Calibration Issue -> with Poweder Coated Sheet
Any advices or tips :)?