Notifications
Clear all

Ugly seams on XL  

  RSS
MartinD
(@martind)
Estimable Member
Ugly seams on XL

I am printing with 0.32 Quality on XL with 0.6 nozzle, material is PETG, all I got is always this ugly seams no matter what kind of boxes I want to print, is there anything I can do with that?

Posted : 17/12/2023 8:45 am
Keno liked
stephan.ribbrock
(@stephan-ribbrock)
Active Member
RE:

That looks nasty. Did you print a heat tower? Perhaps you have to change the temperature a little bit. When I started with my XL I had the impression that it was better for bigger parts as it seemed to be a bit more "rough". Not that it looked that bad. So I swapped to the 0.4 nozzle and it is perfect. It just came to my attention that Prusa is shipping the XL now with the 0.4 nozzle. It is worth a try. When you stick with the 0.6 nozzle you should have a look at the temperature and update your settings.

This post was modified 1 year ago by stephan.ribbrock

Stephan Prusa MK3s+ MMU2S; Prusa XL-1H

Posted : 19/12/2023 10:00 am
Share: