Settings for semiflex or flexfill 98A

Hello,

general settings for semiflex or flexfill 98A have an extrusion ratio of 1.2 (layer higth 0,15) or 1.22 (layer hight 0,2). Is this real?

I use TPU with 98A (Renkforces) and this setting causes the filament to squezze out between hotend and extruder.
This leads to damage (deformation) of PTFE-Tube inlet.

I print this TPU without problems with Standard setting Prusa-Pla, extrusion ratio 1.0!! 225°C, retraction 1,5, retraction speed 150, and bed at 50°C.

Please tell me if this high extrrusion ratio in the Standard-Setting of Semiflex 98A is correct?