Hello
Im using a brand new steel sheet with powder coating (cleaned once with isopropylalkohol), the PETG filament is dried -
but the adhesion is crazy bad.
why?
I'm printing plates, with a big footprint... so adhesion shouldn't be a problem at all...
thanks
RE: adhesion problem
Can you please show us the first layer?
regards Joan
I try to make safe suggestions,You should understand the context and ensure you are happy that they are safe before attempting to apply my suggestions, what you do, is YOUR responsibility. Location Halifax UK
RE: adhesion problem
Did you adjust live z? Textured and satin sheets are about 0.4 mm thinner than plain steel sheets. Also, I'd give the sheet a good rinse with hot water and dish washing soap to remove any residues.