Thanks. That all makes sense. I did dry it for 8 hours@80c, ... Im Forum How do I print this? (Printing help) |
Vor 3 months |
|
PC CF horizontal layer ripples Im Forum How do I print this? (Printing help) |
Vor 3 months |
|
Groaning sound when moving along Y axis Im Forum Hardware, firmware and software help |
Vor 6 months |
|
The bottoms actually look pretty good, and all of them were ... Im Forum Hardware, firmware and software help |
Vor 7 months |
|
PETG - poor quality on textured sheet (1st layer is OK) Im Forum Hardware, firmware and software help |
Vor 7 months |
|
.1mm V6 nozzle? Im Forum User mods - OctoPrint, enclosures, nozzles, ... |
Vor 7 months |
|
I figured it out. I had completely forgotten that I had inst... Im Forum Assembly and first prints troubleshooting |
Vor 8 months |
|
Blobs and scorch marks on otherwise perfect first few layers Im Forum Assembly and first prints troubleshooting |
Vor 8 months |
|
Error # 10109 - too much resin error, when the resin is well... Im Forum Hardware, firmware and software help |
Vor 2 years |
|
Got it - Aligned Rectilinear fill gives me what I need. thx... Im Forum PrusaSlicer |
Vor 2 years |
|
Unable to change fill angle Im Forum PrusaSlicer |
Vor 2 years |