RE: first layer issue
Was this with input shaper? Generic pla with input shaper first layer is like 230 which is pretty hot but non input shaper is 215. I would try bump it to 220 first layer and see how that goes. If youre already at 230 with input shaper then yeah idk, i wouldnt go higher. Confusing indeed, it did so well until that point
RE: first layer issue
Hello sir.
Thank u for ur message. After following ur suggestion, the issue got resolved. May I ask was the reasoing behind ur suggestion? Noob here, hehe.
RE: first layer issue
I suspect the poor adhesion is partly due to a fingerprint.
I wash my build plate with dish soap and water. Then rinse well with hot water and dry immediately with plain paper towels
I also run my heat bed at70C for pla prints.
I try to make safe suggestions,You should understand the context and ensure you are happy that they are safe before attempting to apply my suggestions, what you do, is YOUR responsibility. Location Halifax UK